海水每下潜 10 米约增加 0.1MPa(1bar)。1000 米约 10MPa,3000 米约 30MPa,6000 米接近 60MPa——相当于每平方厘米压上 600 公斤。所有耐压设计、密封与结构强度都从这个数字出发。Every 10 m of seawater adds ~0.1 MPa (1 bar). 1,000 m ≈ 10 MPa, 3,000 m ≈ 30 MPa, 6,000 m ≈ 60 MPa — about 600 kg per cm². Every pressure, seal and structural decision starts here.
两条技术路线Two Design Routes
耐压壳体:金属圆筒承压,电芯置于常压舱内,可靠性高、便于维护,但重量与体积大;Pressure hull: metal cylinder keeps cells at 1 atm — reliable and serviceable but heavy;
充油压力平衡:软包/圆柱组浸在绝缘油中,外部压力经油传递,内外压差接近零,重量轻、形状自由,但对油品、密封与膨胀管理要求高。Oil-compensated: cells immersed in dielectric oil, near-zero differential pressure — light and shape-free, but demanding on oil, seals and swell management.
密封细节决定成败Sealing Details Decide Everything
双 O 圈 + 端面沟槽设计,压缩率控制在 20–30%;Dual O-rings with 20–30% compression;
水密接头优先选成熟型号(如 SubConn 类),每个接插件单独做压力测试;Use proven watertight connectors and pressure-test each one;
灌封胶与金属/塑料的膨胀系数要匹配,避免温循开裂;Match potting CTE to housing materials;
壳体材料:6061 铝合金 + 硬质阳极氧化,或钛合金用于长期浸泡。6061 aluminium with hard anodising, or titanium for permanent immersion.
热与自放电:水下的隐形杀手Heat and Self-Discharge: The Silent Killers
水下散热其实比空气好,但密封舱内热量出不去,需做舱内导热设计;Water cools well, but heat cannot escape a sealed pod — design internal conduction;
长期浸泡设备必须做 K 值(自放电)筛选,剔除微短路电芯;Screen K-value (self-discharge) to reject micro-short cells;
充油结构需预留油体积随温度变化的补偿空间。Oil-filled packs need volume compensation for thermal expansion.
验证:三重测试Validation: Three Tests
压力舱保压测试(1.25–1.5 倍工作压力,保压 2 小时以上);Pressure-chamber test at 1.25–1.5× working depth;
氦质谱检漏,灵敏度到 1×10⁻⁹ Pa·m³/s;Helium leak detection to 1×10⁻⁹ Pa·m³/s;
整机浸泡与温循循环(如 -10℃~40℃ 各 10 次)。Immersion and thermal cycling (e.g. 10 cycles -10 to 40℃).